Dileep
Just consider @40Amps per mm of filler wire. My be between 110 to 130amps depends on passes which pass you are doing. Also see Manufactureer brand packet
recommandation.
 
Regards
Rakesh Kasera
From: Dileep Sankar <dileepsan.08@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, 29 June 2013 8:40 AM
Subject: [MW:18043] Welding in 3G position

Dear ALL,
I would like to know the best parameters to be followed for optimum result in welding an ordinary 3G joint, with E6013, 3.15mm electrode. I would like to know the preferred current (Amps) while welding both the upward and downward direction.

Please help me out.


With thanks in advance,
Dileep Sankar
dileepsan.08@gmail.com
+919787090121
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...