Mazlan,
Can you please give more details in the product?
SV

--- On Wed, 17/4/13, mazlan abd aziz <mazlanaziz66@gmail.com> wrote:

From: mazlan abd aziz <mazlanaziz66@gmail.com>
Subject: Re: [MW:17453] INSULATION PAINT
To: materials-welding@googlegroups.com
Date: Wednesday, 17 April, 2013, 8:55 PM

Dear David,
Yes there is! But I do not know up to what limit it can insulate the
electrical current. For underground piping we are using the fusion
bonded epoxy paint.With 300 micron thickness it can stand 1.5 KV .

On 4/17/13, Chan, David <David.Chan@exterran.com> wrote:
> Hi Subject Matter Experts (SME)
> I would like to seek information on whether such paint exists where the
> Insulation Paint does not permit the passing through of electrical current
>
> Thank you in advance for your feedback
>
> Thank you
> Best Regards
>
> David Chan
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>


--
Best Regards

Mazlan Abd Aziz
Freelance Inspector
Email: mazlanaziz66@gmail.com
          mazsp66@yahoo.com
Mobile:+6019-4772079

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...