sir
    according to ASME Sec IX. for welder qualification maximum  thickness range   is limited ,minimum no problem under  maximum range of qualifcation & wps is guidance  for welder not for limit his qualifcation but welder most be qualified within the essential variable  range(welder perfomance qualification test) of that WPS.
 
Thanks & best regards.
Mohammad Jawed Anwar .
(welding inspector)
Mob no #  +966569799776.


On Tue, Apr 23, 2013 at 1:43 PM, Krish.Saravanan <sarav91@yahoo.com> wrote:
Dear Experts
 
Welder qualification qualified thickness range under ASME Sec IX.
Only maximum qualified weld metal thickness limit given in QW-452.1(b). Is there any minimum thickness limit? Or the minimum thickness is as per WPS which is to be used for production weld? Please advice ….
 Thanks & Regards
Krish
 
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...