Dear sir
For C and C-Mn steels it is possible to make satisfactory welds
without back purge.But normally in this type of situations the line
has to be purged with CO2 or NITROGEN before going to a hot work
operation.but during socket welding it is permissible to prevent the
fire at normal pressure.
On 2/28/13, Dinesh <som.din@gmail.com> wrote:
> Dear sir,
>
>
>
> Please can you verify in project specification for co2 purging on GTAW
> process
>
> .As well need, might be this occurrence of co2 purging to avoid an any
> oxidizer to help in it to catch fire during welding.
>
>
>
> regards
>
> Dinesh
>
>
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Vino Varghese
> Sent: Thursday, February 28, 2013 7:34 AM
> To: materials-welding@googlegroups.com
> Subject: Re: [MW:16892] CO2 purging during TIG welding of CS service line
>
>
>
> Dear Sir,
>
>
>
> What does your WPS states?
>
>
>
> Regards, Vino
>
> On Thu, Feb 28, 2013 at 5:52 AM, K.M Hrishikesan <hrishikm07@gmail.com>
> wrote:
>
> Our safety team recommends CO2 purging during repair welding of a 2" socket
> weld joint of a CS line( consumable- ER 70S-2 process GTAW). Traces of
> oil
> and toxic gases have already been removed from the loop by flushing and
> CO2 purging. Still, as a precautionary measure, CO2 puging is being
> recommended during welding also
>
>
>
> Does it have any impact on the weld quality?
>
>
>
> Thanks
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> <mailto:materials-welding%2Bunsubscribe@googlegroups.com>
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=
> <http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk
> =anet_ug_hm> &gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com
> <mailto:materials-welding%2Bunsubscribe@googlegroups.com> .
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=
> <http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk
> =anet_ug_hm> &gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment