Tuesday, February 19, 2013

[MW:16816] RE: 16801] SWPS

SWPS – standard welding procedure specifications

 

Not the same as AWS D1.1 – Section 3, prequalified .

 

AWS had a program years ago to collect WPSs and PQRs from industry with the intent of writing WPSs that have been tested and proved out by PQRs many, many times by the  welding community.  These WPS’s if followed exactly were proposed to be acceptable without any additional qualification;  i.e. for the conditions stated eliminating the need for PQRs.  There are many more AWS SWPSs than are permitted by ASME.  The subset of permitted SWPSs is listed in ASME Sc IX, Appendix E.

 

Copies of the SWPSs may be purchased from AWS:   http://pubs.aws.org search on the acronym SWPS and you will get a list of available SWPSs.

 

You will find that while they are not inexpensive ($248.00 each), they cost less than making procedure qualification test plates and having the required testing performed.  However, the ASME permitted SWPSs  are very limited in scope.  Per Sc IX SWPSs may not be modified or combined with other WPSs/PQRs – See Sc IX QW-450.

 

My own personal view is that my suspicions are aroused as to the competence of a company trying to employ these.  In over 30 years of reviewing welding documentation (WPSs, PQRs, etc.) I have only seen 1 or 2 companies that employed them for ASME Code work.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ri@z
Sent: Monday, February 18, 2013 11:33 PM
To: materials-welding@googlegroups.com
Subject: [MW:16801] SWPS

 

hellow masters,

 

What is this SWPS means..??

 

Is it possible to purchase SWPS from ASME??

 

With regards

 

Riaz

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...