Re: [MW:16614] Stress relieving & Oxidation on titanium PQR

Hi!
Why did you go for PWHT of Titanium ? if the PQR is on Ti. Generaly Ti does not call for PWHT
Regards
Hegde p.B.

--- On Mon, 28/1/13, Prasu Cutie <pracuty@gmail.com> wrote:

From: Prasu Cutie <pracuty@gmail.com>
Subject: [MW:16609] Stress relieving & Oxidation on titanium PQR
To: materials-welding@googlegroups.com
Date: Monday, 28 January, 2013, 1:16 PM

Dear Experts,

I have Qualified PQR with below deatils

Material: Titanium
Process: GTAW
Heat treatment done twice one is for stress relieving (600deg.C, 1hr soaking, furnace cooling) & other is for Oxidation( 750deg.C, 3hrs soaking, furnace cooling) on same PQR test cupon as per ASME sec.IX

Now my question is, can i write two WPS with separate HT's by having back up of above PQR

as one is with stress relieving & other is with Oxidation.

Request to send me the reply at the earliest with some back up like referance documents if any


Regards
Prasu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...