Sunday, January 13, 2013

Re: [MW:16503] Reg - Thermal Spray Aluminum instead of Galvanizing


Mr. Selvaraj
the only limitation is the profile and access for the ARC spray torch, if the specifications allow flame torch can be used.
But TSA needs a sealer coat and procedure qualification to mee the strenght requriements.
Cost is an important factor for TSA.
 
regards
Gurmeet
On Wed, Dec 19, 2012 at 11:16 AM, Selvaraj.M <selvaraj.m@madinagulf.com> wrote:

Dear Experts,

Can anyone one advise me what will be the limitation of using Thermal Spray Aluminum instead of galvanizing.

 

Best Regards,
M.Selvaraj           
QC Manager
Madina Group|Doha- Qatar|  Ë +974-33199520  É +974-44600818-Ext-238 | selvaraj.m@madinagulf.comü www.madinagulf.com
"Quality leads to business growth through reputation"

 



This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...