Dear Experts,
I have Qualified PQR with below deatils
Material: Titanium
Process: GTAW
Heat treatment done twice one is for stress relieving (600deg.C, 1hr soaking, furnace cooling) & other is for Oxidation( 750deg.C, 3hrs soaking, furnace cooling) on same PQR test cupon as per ASME sec.IX
Now my question is, can i write two WPS with separate HT's by having back up of above PQR
as one is with stress relieving & other is with Oxidation.
Request to send me the reply at the earliest with some back up like referance documents if any
Regards
Prasu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...