Many thanks,
The issue is to verify the overlap itself between some bottom plates, since the owner has some doubts and wants to know if the 5 times the bottom plates thickness is there.
BR

Sent from my iPad

On Dec 31, 2012, at 8:02 AM, "amit sunaria" <amit_sunaria@rediffmail.com> wrote:

Dear friend,

You can use Vacuum Box Test Method for Overlap weld joints.



Thanks & Regards,

Amit,
Inspection Engineer,
ABSIV,Bhogat Terminal,
Jamnagar,Gujarat.



From: Lassaad <lassaad.mokrani@gmail.com>
Sent: Mon, 31 Dec 2012 09:38:54
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: [MW:16377] TANK BOTTOM PLATES OVERLAP
Dear Experts,
Is there any NDT method to check the overlap of bottom plates of an API650 built and used Oil steel tank.?
Many thanks
BR

Sent from my iPad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...