Re: [MW:16384] Final welding appearance

I agree with QC dept This uneven portion require to be welded in taper matching with thicker joint As this sharp joint becomes the stress concentration may cause failure in service
Regards
 
Hegde P.B.
Consultant (Welding Engg)

From: Samir Mehta <samirmehta.jnd@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, 30 December 2012 10:47 AM
Subject: Re: [MW:16376] Final welding appearance
Pls find the attached pic. and advice as the spool is hold by quality control dept, they want me to fill the taper area, and i am not agreed cos its not bevel, pls provide some proof. 
On Sat, Dec 29, 2012 at 7:05 PM, sreekanth <forusree99@rediffmail.com> wrote:

sir,


method -1 is correct as per asme sec ix



Regards,
srikkanth




On Sat, 29 Dec 2012 13:37:52 +0530 wrote
>Dear all,kindly go through the attached file and advice which one is correct and acceptable method as per the welding standard also provide reference documents.regardssamir-- >To post to this group, send email to materials-welding@googlegroups.com>To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com>For more options, visit this group's bolg at http://materials-welding.blogspot.com/>http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm>>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.>>>

Catch India as it happens with the Rediff News App. To download it for FREE, click here
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.  
--
Samir Mehta
Engineer - Welding & Projects
JPIOS
Abu Dhabi - UAE
+971 55 94 25 327
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.  

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...