Sunday, December 30, 2012

Re: [MW:16376] Final welding appearance

Pls find the attached pic. and advice as the spool is hold by quality control dept, they want me to fill the taper area, and i am not agreed cos its not bevel, pls provide some proof. 

On Sat, Dec 29, 2012 at 7:05 PM, sreekanth <forusree99@rediffmail.com> wrote:

sir,


method -1 is correct as per asme sec ix



Regards,
srikkanth




On Sat, 29 Dec 2012 13:37:52 +0530 wrote

>Dear all,
kindly go through the attached file and advice which one is correct and acceptable method as
per the welding standard also provide reference documents.
regardssamir



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

>

>


Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Samir Mehta
Engineer - Welding & Projects
JPIOS
Abu Dhabi - UAE
+971 55 94 25 327

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...