Re: [MW:16356] Grinding or filling is allowed on Final pass (on capping) for WPQT ? Urgent plse..

ASME Sec IX do not address this issue.

As far as I know, the only code which allows grinding of completed welds is AWS D1.5 - 2002 (Bridge Welding Code)  See Clause 3.2.2.1, 2nd para, Point # 4.
(4) grinding the completed weld smooth and flush with the adjacent surface
to produce a workmanlike finish (see 3.6.3).


Further, 3.6.3 says : Unless otherwise approved by the Engineer, all reinforcement
shall be removed where the weld forms a part of a faying surface. Any reinforcement shall blend smoothly into the plate surfaces with transition areas free from weld edge
undercut. Chipping may be used, provided it is followed by grinding.

IMO, grinding of the completed welds should be applicable only for ( including as suggested by C Sridhar) removing sharp notches, bulbous contours, overlaps only with prior approval and presence of concerned Inspector/Engineer, especially qualification welds.

No welder should be allowed to grind the completed welds on their own, as they make it mess sometimes. I have seen welders try to "remove" external undercuts by grinding the base metal and bringing it to the level of surface of undercut, which may reduce the minimum specified wall thickness of the base metal.

Filing a completed weld for good visual appearance, is not a problem, I think.

I'm also waiting for opinion of the experts of this forum.  

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Thu, 27/12/12, c sridhar <sridhar305@yahoo.com> wrote:

From: c sridhar <sridhar305@yahoo.com>
Subject: Re: [MW:16353] Grinding or filling is allowed on Final pass (on capping) for WPQT ? Urgent plse..
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Thursday, 27 December, 2012, 4:43 PM

Mr. Sathis kumar,

Codes do not specify about the grinding & filling, on not only final but even in filler passes. It is the discrepancy
of the Inspection authority who witnesses the test. Some allow it while few do not. They feel it is lack of skill on the part of the welder concerned if he is allowed to grind such surface defect.

But, it need not be a fact. Say  if it is a surface pore due to sudden breeze or to other reasons where welder is not at fault, he takes the Inspector into confidence to remove such defects by grinding or other means.  So it is a selective thinking.

More attention is given in initial visual inspection for root defects like. LP, LF, UC,  Ex. Penetration , Oxidation (in TIG process), Cavities, under flush etc., than on surface defects on cap runs.

Sridhar.

From: Sathish Kumar <sathishbemech@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 27 December 2012 2:37 PM
Subject: [MW:16349] Grinding or filling is allowed on Final pass (on capping) for WPQT ? Urgent plse..

Dear Experts,
Please advice.
whether Grinding or filling is allowed on Final pass (on capping) for Welder performance qualification test (WPQT) for Plate or Pipe. Since qualification is done based on ASME Sec 9, so i need reference only as per ASME Sec 9.
Also already i referred ASME Sec 9 - QW194, which only mentions the Complete joint penetration for visual examination for WPQT. But it is not more specific in case of Grinding or filling and also some other (acceptable limits ? )parameters like Reinforcement, undercut, underfill etc..
I need only Asme Sec 9 reference, because as per the project contract only Asme Sec 9 is applicable for our project in case of WPQT.
please advice guys..
Thanks in advance..
 
Regards
sathish. K
Welding inspector.
Jubail, Saudi arabia.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...