Monday, December 24, 2012

Re: [MW:16313] AWS E347-15 E347-16 Stainless Steel Welding Rod

1. E347-15 will have better penetration than E347-16 but 15 is difficult to handle than 16. mostly 16 is used for surfacing and finish is superior than 15
Pandithan
Welding Consultant

On Sat, Dec 22, 2012 at 12:24 PM, welding <samirmehta.jnd@gmail.com> wrote:
Dear Expert,

Wt reference to the subjected matter, kindly provide the difference between E347-15 and E347-16. as initially we were using E347-15 and it working good but now we hv changed to E347-16 and our welders are starts complaining ab the quality of electrode. pls advice if it need some other Technic to weld or parameter variation. 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...