Friday, November 30, 2012

Re: [MW:16086] EN 8 EN19 EN24 welding

Hi,
You can Use E7018 for EN8 and E9018 for EN19 and 24.
Please find herewith the attached file might be useful to you.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282

From: "pankaj.kolhe@wipro.com" <pankaj.kolhe@wipro.com>
To: materials-welding@googlegroups.com
Sent: Thursday, November 29, 2012 2:30 PM
Subject: [MW:16071] EN 8 EN19 EN24 welding

Dear all,
Can anybody tell me regarding the consumable to be used for EN-8,EN19,EN24  to SA 516 Gr 70 and SA 106 Gr 70 and SA335  welding and EN8,EN24,En19 to self welding.
 
Regards
Pankaj Kolhe
QC Dept.
Wipro Limited (Wipro Water)  
Serene Properties Private Limited, SEZ, Plot No. 3, Building No. 7, 6th Floor, TTC Industrial Area, Thane-Belapur Road, Airoli, Navi Mumbai – 400708, Maharashtra, India.  Tel- +91 22 39302135   E-mail- pankaj.kolhe@wipro.com 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

[MW:35692]