[MW:15827] PQR with Filler wire ER316L Flux SA Cs2 Cr DC can e used on SS304L base metal

Dear Experts 

 PQR with Filler wire ER316L Flux SA Cs2 Cr DC; base metal base SA 240 SS316L.

Can we use this PQR to weld base metal SA 240 SS304/304L without changing Flux with 308L filler wire! Or re-qualification is required.

 

Thanks & regards

Ali Mhaskar,

UAE 

 

 

 

                   

 

 