Monday, October 22, 2012

Re: [MW:15741] EXCESS DFT OF PAINT

Vinu,
The specified DFT will probably be a minimum, you are supplying
More corrosion protection than is required,
Your client may be quite happy with this,
Why don't you ask them. It is better to have too much
Than not enough

Declan

Sent from my iPhone

On 22 Oct 2012, at 10:35, kumar mahesh <chichulamaheshkumar@gmail.com> wrote:

Dear Vinu

As the DFT increases it will lead to cracking  if the particular substrate is under going for bending

On Mon, Oct 15, 2012 at 3:10 AM, manpreet <manpreetsin88@rediffmail.com> wrote:
Hi Mate,

ISO 12944-5 Sec 5.4 states that "It is recommended that the maximum dry film thickness (individual value) is not greater than THREE TIMES the nominal dry film thickness."

Do some tests such as adhesion test and solvent rub test.

Cheers.


On Sun, 14 Oct 2012 14:39:23 +0530 wrote
>Dear Friends!I would like to know if there is any problem in DFT of paint which is actually 2 times the specified DFT. And how do i correct this problem.? Should i remove the paint?


--
VINU RAVEENDRAN




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>

>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

>

>


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Chichula Mahesh Kumar
+91 9700081617

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...