Tuesday, September 25, 2012

Re: [MW:15394] Welding consumable for welding of CS to Cast Iron

Dear All,  That's the correct recommendation,  I have seen many times in this forum people misusing the forum to abuse other's products and promote their products especially some so called "REPUTED " companies.

Hats off to Mr.Saleem for giving a codified product as solution than giving a brand & promoting it.

J.Srinivasan



On Tue, Sep 25, 2012 at 7:05 PM, hesham seleem <heshamseleem7@hotmail.com> wrote:
Dear Sir

Regarding To Your Question about welding CS to DI-Electrode Used is

AWS A5.15: ENIFe-c1

DIN 8573: ENIFe-1  BG13



Date: Tue, 25 Sep 2012 17:36:01 +0530
Subject: [MW:15391] Welding consumable for welding of CS to Cast Iron
From: ranendrac6@gmail.com
To: materials-welding@googlegroups.com


Dear Experts,
Please guide which kind of consumable can be used for welding of CS with Cast Iron.
 
Ranendra Chakraborty

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
J.SRINIVASAN

GENERAL MANAGER - TRAINING

D&H SECHERON - INDORE

Mob: 7898989756

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]