Re: [MW:15365] Consumable storage in AC room

Dear Naresh,

As per my opinion , it is totally unacceptable.  


Thank you.

On Sat, Sep 22, 2012 at 7:02 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:
Dear experts,

Whether welding consumable storage in air-conditioned (AC) room is acceptable,including low hydrogen and SS electrodes. Ex: E9018-B9,E7018-1,E316L etc.,
 
Thanks & Regards,
Naresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--




With kinds Regards

*********************

PRAVEZ ALAM

MATERIAL/PIPING INSPECTOR

SK E &C

Ruwais Refinery Expansion Project, 

P O Box : 11780, Ruwais,  Abudhabi.

United Arab Emirates.

Mob-+971509867435

E-mail-skec.cv4087@partner.sk.com

            alampravez@gmail.com


"When I am working on a problem I never think about beauty. I only think about how to solve the problem. But when I have finished, if the solution is not beautiful, I know it is wrong."



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...