Wednesday, August 29, 2012

Re: [MW:15154] PWHT OF T91

Mr. Shiva,
The recommendePWHT  Temp. for SA 213 T91 is  720 to 760 deg. C  
Hence 740 deg.C should not pose any problems.
sridhar.
---------------------------------------------------------------------------------------------------


From: boom shiva <boomboomshiva122@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, 28 August 2012 4:13 PM
Subject: [MW:15143] PWHT OF T91

what effect would be there if SA213 T91 tube is PWHT at lower than 760 deg. C? suppose 740 deg. C?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...