Hi,
I have a qualifed a PQR for 18mm PLATE P1 to P1, also tested for Charpy test for -40 deg (just in case for future use) I have a request to know,
 
1. What will be the thickness limitations if I were to develop a WPS where Charpy Test Requirment would be involved. Also is there any Preheat requirement and if so above what thickness?
 
2. I am developing a WPS for welding and without Charpy Test requiremnt, I believe the thickness limitations using the PQR would be 5 to 36mm.
 
Your advise would be highly appreciated

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...