Thursday, July 19, 2012

Re: [MW:14898] welding of dissimilar material CS SA106 to SS 316

Since your WPS done for SA 333 Gr. 6 to SA 312 TP 316 is grouped under
P1 Gr 1 (vs) P8 Gr 1. no need to do new WPS as new materials also falls
under same P1 Gr 1 (vs) P8 Gr 1.

you can use the earlier  WPS for your present  dissimilar welding also.

sridhar


From: Tiger <ezatadel2008@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 19 July 2012 12:40 AM
Subject: [MW:14894] welding of dissimilar material CS SA106 to SS 316

Dear Exprets,
 
 i have a fillet weld of dissimilar material CS SA106 to SS 316 but i don't have WPS , also i have WPS for CS TO SS ( A333 GR6 P.1 to A312 TP316 P.8 ) if it is applicable to use it for the other material.
 
thanks,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...