Tuesday, July 24, 2012

[MW:14944] RE: 14932] VERTICAL VESSEL INSULATION

          Insulation can be done by using cleats or round bar after that aluminum coil or SS sheet can be used to hold the Insulation material.

 

 

          Regards

 

          M.G.Kattiomani

 

 

 

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lassaad Mokrani
Sent:
Monday, July 23, 2012 5:09 PM
To: materials-welding@googlegroups.com
Subject: [MW:14932] VERTICAL VESSEL INSULATION

 

Dear Experts,

We have a SS vertical vessel for which we need to make insulation for Personel Proetction reasons.

Having a skirt welded around in its base, it looks confusing how to apply the insulation material knowing that its bottom is as well dish ended and fitted with Heat tracing cable. (see DSH).

Do you have any recommendation??

 

Thanks

 

--

Meilleures salutations

MOKRANI Lassaad

Consultant Civil Engineer

Tunisia

00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907


















P     Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail



















P     Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail


This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...