Dear expert,

As per ASME 8-1-UCS-56

We have done SR for our 40mm thk-30" pipe joint.

but unfortunetly, soaking time was just short by 5min.Now our client/PMC both are not agree to release.

Required time : 1hr.15min
Actual Time : 1hr.10min

It is acceptable OR could you share any technical view to convince client?

regards,
mohd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.