RT / MPI before PWHT is internal inspection and RT / MPI after PWHT is
required by ASME B.31.3 para 341.3 Examination requirements,
(a) for P.nos 3,4 and 5 materials Examination shall be performed after 72 hours
completion of any heat treatment.
--
George Xue (Xue Guoliang)
Suzhou CXGL Mechanical Engineering Co., Ltd.
Purchasing and Engineering Manager
Rm 418 No.979, Sanxiang Road, Suzhou, 215004, Jiangsu,China
Tel: +86-512-68639769 Fax: +86-512-68639492
Email: cxueguoliang@gmail.com
Skype: xuegl2001

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...