Dear friends,
we recently changed the ethane furnace tubes after service in 4 years,
now we are planning to segregate the healthy tubes & return bends
from used/removed lot to re-use in future if needed. Material of the
tube/bend is 25Cr/35Ni/Nb+Micro.
We can check visually for cracks, thinning, bowing etc. UT is not
feasible, because there is some sort of rough coating over it.
How about the field metallography for carburization?
thanks a lot to all dear friends.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment