[MW:14673] Storage Conditions of Welding Consumables.

Dear Experts,

Kindly Provide Your Valuable View on Below Queries.

1. What is Recommended Procedure / Conditions for storage of MMA electrodes, SAW Wire Spools, TIG Wires & SAW Fluxes in term of Consumable Storage Room Temperature Relative  Humidity?


2. What to do if we could not maintain the Required Consumable Storage Room Temperature and Relative Humidity


Thanks & Regards


Tariq Hussain 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...