Hi Vinod,
Generally austenitic stainless steels are very popular materials in
pharmaceutical industry due to hygiene and cleanliness issues. The selection
may vary from 304L 316L/LN and to the higher ends also.
Alternative could be duplex S.S also(see as attached).
The other options could be fluoro-polymers.But this is fairly new area in
terms of MOC.(seethe DuPont article)
I would think based on the operating parameters presented below a choice
between austenitic S.S or duplex could be ideal.
Thanks.
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Aniket Gupta
Sent: Tuesday, May 22, 2012 4:13 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14337] MOC for High H2S gas under pressure
You can use Carbon Steels with Nace Quality ( Controlled Composition of
Alloys).
Ex SA 516 60 ( Nace for Sulphide Cracking) Some of the clients want Heat
Treatment after fabrication.
Aniket Gupta
On 5/20/12, vnbhatt@gmail.com <vnbhatt@gmail.com> wrote:
> Respected Material Experts,
>
> We have a pharmaceutical client inquiry where they have gas media with
> 60 % H2S gas in the mix with 500 PPM moisture flowing from piping,
> vessels and shell-tube exchanger under pressure of 37 bar gauge.
>
> With many experienced brain on group, I seek details as to what MOC to
> be employed, what quality checks and what corrosion allowance??
>
> Appreciate guidance.
>
> Regards,
>
> Vinod Bhatt
> Sent on my BlackBerryR from Vodafone
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment