uneven coating or flux coating not concentric, try with different
brand
On May 29, 5:03 pm, murtaza...@yahoo.com wrote:
> I have a MMA welding electrode of SS 308L Dia. 2.6mm. when half of
> the electrode is consumed it get red hot, and it gives porosity in the
> weld metal what could be the reason i.e. is it a welding problem or
> there is a problem in the electrode???
> if this problem is due to electrode then what can be the reasons and
> rectifications???
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
brand
On May 29, 5:03 pm, murtaza...@yahoo.com wrote:
> I have a MMA welding electrode of SS 308L Dia. 2.6mm. when half of
> the electrode is consumed it get red hot, and it gives porosity in the
> weld metal what could be the reason i.e. is it a welding problem or
> there is a problem in the electrode???
> if this problem is due to electrode then what can be the reasons and
> rectifications???
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments