Dear friends,
We are doing welding (GTAW using 99.99% Argon & 70-30 cnsumable) of
CuNi - 90-10 pipe and all of them fall under class 1 pipe and forced
to examine the weld by Radiograpy. On review of radiograph, none of
the joint gets cleared. The only problem with welding is "POROSITY".
As pe our contract, the size of permissible porosity is 0.2t
(thickness of pipe is 3,4mm) and even 1mm porosity calls for repair.
Could any one share your knowledge on the following.
1. Acceptance criteria for RT of CuNi pipe weld
2. How to overcome from the porosity
Best Regards,
Megnath
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment