Thursday, April 19, 2012

Re: [MW:14125] suitables electrode used for cast iron

U can use
 
1)  EutecTrode 27 for Base layer
 
2)  Xuper 2240 for final layer
 
with best rgds
= s p raman=
 
----- Original Message -----
 
 
Sent: Tuesday, April 17, 2012 3:09 PM
Subject: [MW:14117] suitables electrode used for cast iron

Hi experts,

I need your help. I prepared procedure to welding panama chock (cast iron material)  to high tensile strength plate (EH 36). what is the suitable eloctrode to used for smaw process? can i used the  ordinary low hidrogen eloctrode such as KOBE brand E 7018? or special elctrode? please advice me.

Thank you.

Ezzudine Must.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...