Dear Hilman,

As per ASME VIII Div.2 clause 8.2.5 stated any leaks that are present, except for that leakage that may occur at temporary test closures for those openings intended for welded connections, shall be corrected and the vessel shall be retested.

So if your pressure vessel which repair area fully radiographed and the result is acceptable I think your vessel shall be retested.


Regards,



Lukman
Sent from my BlackBerry®
powered by Sinyal Kuat INDOSAT

From: Himan Nikdin <himannikdin@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Mon, 16 Apr 2012 10:59:34 +0430
To: materials-welding Group<materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:14110] welding after hydrostaic test

Dear experts
 
I would appreciated if anyone can share some refrence (code) regarding allowance of welding after hydrostatic test on pressure vessle which repair area fully radiographed and the result is accepatble.
 
Regards,
himan Nikdin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...