Dear Dhamothran,

As per API 650 para 4.5.2 stated material for shell nozzles and shell manhole necks shall be seamless pipe, seamless forging or plate material as specified in 4.2.9.1.

Regards,

Lukman
Sent from my BlackBerry®
powered by Sinyal Kuat INDOSAT

-----Original Message-----
From: Dhamotharan <dhamu.prowess@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Tue, 17 Apr 2012 02:12:50
To: Materials & Welding<materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:14116] Nozzle neck fabricated by welding plate as per API 650

Dear Experts,

As per API 650, is it allowed to prepare a nozzle neck of 16" Dia by
rolling a plate of 6 mm thickness?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...