Monday, April 16, 2012

RE: [MW:14112] welding after hydrostaic test

Dear Mr.himan,
welding after pressure testing is not acceptable. Before hydro test the line clearance to be made which includes welding, repair welding if any, NDT clearance, PWHT and all other punch list related to welding. After hydro test, only painting and insulation could be carried out.

Sent from Nokia C7 phone
-----Original Message-----
From: Himan Nikdin
Sent: 16/04/2012, 10:29 AM
To: materials-welding Group
Subject: [MW:14110] welding after hydrostaic test


*Dear experts*
**
*I would appreciated if anyone can share some refrence (code) regarding
allowance of welding after hydrostatic test on pressure vessle which repair
area fully radiographed and the result is accepatble.*
**
*Regards,*
*himan Nikdin*

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...