Friday, April 6, 2012

RE: [MW:14073] defects in Radiographic interpretetion - an illustration

Slag looks wider than undercut and undercut would follow the weld, not be straight – my opinion

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of zakir ali
Sent: Friday, April 06, 2012 2:35 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14070] defects in Radiographic interpretetion - an illustration

 


Dear Sajid,

Root under cut will be darker & more sharp, whereas the slag would be less darker & have hazzy appearnce.

Regards,

Zakir Ali.


From: sajid sakhidas <sajidsakhidas@gmail.com>
Sent: Fri, 06 Apr 2012 11:20:17
To: materials-welding@googlegroups.com
Subject: Re: [MW:14065] defects in Radiographic interpretetion - an illustration

Dear expert,

 

Good afternoon,

 

Any one suggest how to distinguish between root under under cut(RUC) and elongated slag inclusion  during  RT interpretation.

 

Thanks

SAJID

On Thu, Apr 5, 2012 at 10:40 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:


http://www.4shared.com/office/BwNoWtwO/Welding_Errors_.html


---------- Forwarded message ----------
From: Harry Patel <harryeng...@gmail.com>
Date: Nov 2 2011, 4:39 pm
Subject: Welding Defect Photo
To: Materials & Welding


Dear Sirs,

Anybody have welding defect photo like incomplet fusion,incomplete
penetration, root concavity in pipe.

I hope for your reply.

Thank you very much in advance.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...