[MW:14110] welding after hydrostaic test

Dear experts
 
I would appreciated if anyone can share some refrence (code) regarding allowance of welding after hydrostatic test on pressure vessle which repair area fully radiographed and the result is accepatble.
 
Regards,
himan Nikdin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.