Re: [MW:14032] Renewal &Continunity of welder qualification

Dear Friend,
           as per my understanding the welder should be renewed with NDT report. and that NDT report shall be signed by any client for evidence. we have to attach the report with the welder performance record and renew with date of renewal and date of next expiry.
Actually speaking we have to maintain welder history record. from that any client could understand this welder is capable to give good weld. i hope u could catch me. thank you.



--
Regards,
J.C.Andrews
Sr.QA/QC
Bahrain




On Thu, Mar 29, 2012 at 2:00 PM, yahya albalushi <qci.y.albalushi82@gmail.com> wrote:
Gents,

For the welder who has been doing production weld for the last 6
months since his qualification test,Where his company keeping his
performance record.what are the required continuation documents to be
provided to the client in each 6 months? overmore, does his WQT record
needs to be renewed by means of getting stamp of clients QC to
validate his qualification?

Regards,

Yahya
QC(PIPING)
Oman

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...