Friday, March 30, 2012

Re: [MW:14025] P-91 material and Welding


Dear Rohit,

Here i have enclosed for Gr.91 forming & welding Tips, as required by you.


On Wed, Mar 28, 2012 at 2:41 PM, Rohit mn <rhmalhotra84@gmail.com> wrote:
Dear Experts...

Can anyone provide me PPT on P91 material and how to perform welding
and what are the special precaution need to be taken.....

rgds
Rohit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,
G.jayaprakash
Alstom Projects India Ltd,
Durgapur.
09679997249

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...