Thursday, March 29, 2012

Re: [MW:14018] Renewal &Continunity of welder qualification

As per my understanding there is no need to get renewal of WQT if the welder still work at the same company of the WQT he attend. only required if the welder work with other company for a duration 6 month above then he needs to get renewal. if you want prove to your client for your welder performance, do PRODUCTION TEST.
On Mar 30, 2012 12:11 AM, "yahya albalushi" <qci.y.albalushi82@gmail.com> wrote:
>
> Gents,
>
> For the welder who has been doing production weld for the last 6
> months since his qualification test,Where his company keeping his
> performance record.what are the required continuation documents to be
> provided to the client in each 6 months? overmore, does his WQT record
> needs to be renewed by means of getting stamp of clients QC to
> validate his qualification?
>
> Regards,
>
> Yahya
> QC(PIPING)
> Oman
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.