Re: [MW:13586] Pipe damaged during fabrication

No, cann't be rectified by buttering  or built-up on pipe for new construction.

On Mon, Jan 30, 2012 at 6:22 PM, jesti fer <jesti_fer@yahoo.com> wrote:
Dear Experts,
I have problem in our site that, we found some fabricated pipes ( as per B31.3) the parent material thickness reduced by grinding (or due to any handling mark) more than 12.5% is not acceptable,
is there any possibility to build up (Buttering) the base metals. Where can I will get the reference
 
jestifer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...