Sunday, January 22, 2012

Re: [MW:13542] Valve Back Seat Test

Dear Mr Gopi,

Some of the valves are provided with backseat features. The backseat features enables the maintenance crew to replace the gland packing even when the system is under pressure. i.e. the valve is opened fully to 100 %  and the conical shape of the stem touches tightly against seat construction ( back seat ) in the valve body which seals off the fluid passing to gland packing area. Thus one can replace gland packing on line.

Vinod


From: Gopi Perumal <parinitaa2010@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, January 21, 2012 12:01 PM
Subject: [MW:13531] Valve Back Seat Test

Dear all,

Anybody can explain what is mean by Backseat test in Valve Testing? (API 598)

Thanks,
P Gopi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...