[MW:13504] Re: Regarding welding consumable for Material hastelloy C276

Hi,
GTAW - A5.14 - ERNiCrMo-4
SMAW - A5.14ENiCrMo-4
 
It can be used for Dissimilar welding also(With Stainless Steel) Pls.find herewith the attached file of Welding Consumable Detail.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: Vivek Pandey <vivek.pande06@gmail.com>
To: materials-welding@googlegroups.com
Cc: pgoswami@sympatico.ca; karthik6684@yahoo.com
Sent: Wednesday, January 18, 2012 12:32 PM
Subject: Regarding welding consumable for Material hastelloy C276

Dear All

With reference to above subject,kindly suggest me which Consumable is
suitable for welding of hastelloy C276 material( UNS NO: N10276 ).
actually I want to do qualify in two different procedure.
preocedure are as follows

Material: UNS NO:N10276+UNS NO: N10276                PROCESS GTAW+ SMAW

Material: UNS NO:N10276 +SA182 GR 316L    PROCESS GTAW+ SMAW