according to ASME sec IX this material falls in 'P' No 1 : you can see
if material to be welded have carbon content more then 0.3% or its
thickness is more then 25 mm it should be preheated 79 degree C in any
other case min temp for welding is 10 deg C i.e no need of pre
heating.REf ASME Sec VIII Div 1 (2010) Non mandatory appendix R. You
can see table UCS-56 of same sec for PWHT.

email me if further help needed.
Take care
ME

On Jan 16, 2:52 pm, jesti fer <jesti_...@yahoo.com> wrote:
> Dear Experts,
>
> I need your help for this subject, We are fabricating some piping as per B31.3, the material ASTM A106 Gr.B, 8"Sch-XXS and 160 and we are doing preheat and PWHT for welding, but my enquiry pre heat is required for cutting also? It is mentioned in any code or any other were? Please help me
>
> Jesti

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...