Re: [MW:12749] RT density

in general practice the required density in the radiographs will be accepted from 2.0-4.0 for gamma rays, and 1.8-4.0 for x-rays. so in standards it is not mentined required range of density for the radiographs overlap, overlap has to be good enough to match the two successive films. in normal practice they will be accepeted for density range of 1.8-3.0

On Thu, Oct 20, 2011 at 7:09 PM, pankaj.kolhe15 <pankaj.kolhe15@gmail.com> wrote:
Dear sir,
what is the density requirement at overlapped area , if the two films
got overlapped
for gamma rays and where it is written

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...