dear Zakaria,
this grade is specially designed for cryogenic application.. additional  requriment    CVN Impact  @ minus oc.
so you can not use as alternative G grade. 
chandrakant 


From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 20 October 2011 2:46 PM
Subject: [MW:12727] May E8018-C1 substitue E8018-G to weld Corten Steel


Hi all

For welding Corten steel, we have in storage E8018-C1 Electrod, may it substitue  E8018-G, how can confirm ?

Regards
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...