Wednesday, October 26, 2011

[MW:12774] RE: PWHT in TP 321

By any chance does your project spec calls for "Stabilization anneal". It's
a post fabrication anneal(850-900 deg C)applied for stabilized stainless
steels to improve the post fabrication corrosion resistance.

If you could provided more details, I could write to more about the pros and
cons of this method.

Thanks.

Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

-----Original Message-----
From: pradip kumar sil [mailto:pradipsil@gmail.com]
Sent: Wednesday, October 26, 2011 2:17 AM
To: materials-welding@googlegroups.com
Cc: pgoswami
Subject: PWHT in TP 321

Dear Everybody,
First of all Wise you a happy diwali to you & your family.
In my project specification says ASTM A 312 TP 321 has PWHT. My question is
why we will do TP 321 needs to do PWHT because this material have high Cr/Ni
as well as Ti.
Regards
Pradip


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...