Friday, October 21, 2011

[MW:12747] RT Requirement

Hi all,

Can you pls help me, we have given order to our vendor in china for making ASME Pressure vessel, they have done 10% RT shot in long seam welding, but they have found crack and they rectify and again and then taken RT is passed and they delivered the item to singapore, but our client has raised concern that we need to RT in two more shot, but it was missing

Is it mention any where in the ASME about the two additional shot?
Which spec say that 10% RT on long seam?

Client never mentioned anything about this requirement, we strictly follow ASME

With regards

Vimal Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...