[MW:12576] MW: 12563- PWHT of modified P460 NL1 (1.8915) EN 10028-3

Hi David,
 
Please recall today's discussion on this subject. ASME Sec-IX is yet to assign any P No to this steel. Some authentic references on nominal composition and mechanical properties are available in this attachment.
 
This material is accepted for design and construction in Sec-VIII, DIV-2 code, through code cases ,i.e CC-2477 (approved June,2005), reapproved  as CC-2594 ,Nov-2007. ASME imposed some restrictions on this steel, e.g:-
  1. thickness of plates not to exceed 20 mm (0.79 in)
  2. max copper in the plate -0.20%
  3. Vanadium, 0.10-0.20%
  4. design temperature not to exceed 150 deg F(65 deg C)
  5. PWHT Temperature range-985-1040 deg F(530-560 DegC),Minimum holding time 1/2 hr(30 min) at this temperature.
You may find more details in the code case.
 
Usually European consumable manufacturers ,ESAB, Bohler Thyssen or Metrode should be in a position to offer the recommended welding products for this steel. As this steel is a HSLA grade, often there may not exactly matching weld metal chemistry. However the consumable supplier definitely will have better idea.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of David Stevenson
Sent: Tuesday, September 27, 2011 5:27 PM
To: materials-welding@googlegroups.com
Subject: [MW:12563] PWHT of modified P460 NL1 (1.8915) EN 10028-3

As this material is not in the tables can anyone provide the PWHT process for material 14.60mm thick in a pressure vessel built to ASME section VIII division 2?

 

THE FIRST CHOICE IN TANK CONTAINERS

DAVID STEVENSON
TECHNICAL MANAGER
Eurotainer U.S. INC.
5810 Wilson Rd. Suite 200, Humble, Texas, 77396 USA
Phone 01 832 300 5019 (Direct)● Mobile 01 713 805 0192 ● Fax 01 832 300 5050

email: dstevenson@usa.eurotainer.com ● website: www.eurotainer.com

 Please consider the environment before printing this document

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...