Wednesday, September 28, 2011

[MW:12563] PWHT of modified P460 NL1 (1.8915) EN 10028-3

As this material is not in the tables can anyone provide the PWHT process for material 14.60mm thick in a pressure vessel built to ASME section VIII division 2?

 

THE FIRST CHOICE IN TANK CONTAINERS

DAVID STEVENSON
TECHNICAL MANAGER
Eurotainer U.S. INC.
5810 Wilson Rd. Suite 200, Humble, Texas, 77396 USA
Phone 01 832 300 5019 (Direct)● Mobile 01 713 805 0192 ● Fax 01 832 300 5050

email: dstevenson@usa.eurotainer.com ● website: www.eurotainer.com

 Please consider the environment before printing this document

 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...