Saturday, August 27, 2011

Re: [MW:12315] RE: 12305] CD4MC4 matraial

The material may be CD4MCu.may be u appears is 4 in handwriting.
pls check.
Muniyandi
DNV

On Sat, Aug 27, 2011 at 9:39 AM, pgoswami <pgoswami@quickclic.net> wrote:
Hello Badri,
 
What's the ASTM or other material specifications related to CD4MC4 material? I did fairly detailed search  on this material without any success. If you could provide more details it would be appreciated.
 
See the attached literature from 2 major foundries, all other grades are cast except this.
 
Appreciate more details from your end.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of khemici badri
Sent: Thursday, August 25, 2011 8:13 AM
To: materials-welding@googlegroups.com
Subject: [MW:12305] CD4MC4 matraial

Hi everyone;
 
I would like to get some information on the CD4MC4 material. Untill now, I just know the CD4MCu duplex stainless steel grade.
 
Any comments are appreciated. Thanks in advance.
 
Badri
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...