What is the joint type...?
Socket weld fittings or thread or but-welding fittings...?

Maybe MIG-Brazing is what you need if your application is sealing threaded joints or socket welded fittings (it doesn't remove the Zinc coating)

For butt welding joints it may be different...


Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
   



On Thu, Aug 25, 2011 at 3:24 PM, naveed ahmed <naveed_aytb@yahoo.com> wrote:
can any body clarify
which filler wire is required for welding galvanized pipe ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...